Synthesis of DMC-based polyether polyol by a continuous method

A certain amount of DMC catalyst is taken and uniformly dispersed in a certain amount of small molecule initiator. Add 0.5kg of the mixture of the initiator in the small test reactor. The vacuum was replaced 1-2 times with N2, and the N2 pressure was maintained at 0.1 MPa.After heating, stirring and raising the temperature to a certain temperature, the quantitative PO was introduced into the continuous autoclave with nitrogen gas for induction. When the induction is successful (the temperature in the kettle rises and the pressure drops), the PO is continuously passed to carry out the reaction. Open the outer loop and continue to pass the PO into the continuous kettle. When the liquid in the reaction vessel is full, the PO, DMC catalyst and the initiator are continuously added to the kettle at a certain ratio and a certain speed through the power system. Continuous discharge is started when a certain pressure is reached in the continuous autoclave. Keep the feed rate the same as the discharge rate until all the stock is added. The crude product discharged from the kettle enters the aging kettle, and is heated, matured, degassed, and discharged to obtain a finished product.

Related Products Wiki
  • What is GLycolic Acid?

    What is GLycolic Acid?

    March 13, 2019We like to focus on the ingredients of beauty products. But we prefer to touch the product and explore whether it really works. Alpha hydroxy acid is also known as AHA. It includes glycolic acid, lact...view
  • 79th API China

    79th API China

    January 31, 2018November 15-17, 2017Xiamen International Convention and Exhibition CenterAPI China is China's leading exhibition for the pharmaceutical manufacturing sector covering the complete spectrum of products ...view
  • Preparation Of Ammonium Iodide​

    Preparation Of Ammonium Iodide​

    August 2, 2019254 g of potassium iodide dissolved in 125 ml of water are mixed with 100 g of ammonium sulfate dissolved in 125 ml of boiling water. After cooling, 40 ml of alcohol are added and the mixture is kept ...view
  • Application of Expandable Microspheres

    Application of Expandable Microspheres

    April 29, 2019Expanded microspheres (also known as foamed microspheres) are high molecular polymers. Its outer shell is made of a high molecular polymer (acrylic eye copolymer) which is a hydrocarbon inside. In the...view
  • Preparation of Ethyl Iodide

    Preparation of Ethyl Iodide

    April 29, 2019Preparation of ethyl iodideFirst, the principle:Ethyl iodide is usually reacted with ethanol, iodine and red phosphorus, but the reaction is slow, and it needs to be heated in a reflux device for seve...view
  • POC2017 Palm & Lauric Oils Price Outlook Conference & Exhibition

    POC2017 Palm & Lauric Oils Price Outlook Conference & Exhibition

    January 30, 2018POC2017 Palm &Lauric Oils Price Outlook Conference & Exhibition 6-8 March 2017 Kuala LumpurThe renowned Palm and Lauric Oils Price Outlook Conference & Exhibition (POC) is held a...view
Related Products
  • TEL:+86-25-52337978
  • EMAIL: info@njchm.com
  • ADDRESS:12/F, Block B, Technology and Innovation Building, Nanjing University of Technology, No.5 New Model Road, Nanjing 210009, China